Function& application:
dark
grey cylinder, it is used for melting and casting, to adjust the Cr content in the alloy, is the
best material
to instead of Al –Cr alloy. Suitable for non-ferrous
metal plate, belt, foil, profile, rod, wire and cable and non-ferrous alloy
preparation, etc.
Character:
0.5
Usage:
1.It can be directly added to
the melting furnace and better to use before refining , molten aluminum
temperature required: 730
2.Make an analysis about metal element on alloy before use, calculate inputs of additive according to demand and additive yield rate.
3.Removal off the packing, put
the additive into the molten alloy evenly , close the furnace door and keep
20-30 minutes, and then stirring for 10 minutes and deslagging.
4. Secondly, adjusting temperature, 10 minutes later, stirring completely again, refining for 15 minutes and deslag to get needed alloy.
Package and conservation
Keep in ventilated and dry
environment.
Guarantee period 12 moths.
Gather package and dispose, no
burning inside stove